Annic KilnYatangiriye mu kinyejana cya mirongo itandatu rw'ikinyejana cya mirongo itandatu, Ubudage, bwahoze azwi ku izina rya PONCKENBACH itanura ry'aho yakorewe akarere, ni ubwoko bw'indirimbo ya lime vertique itanura, hamwe na shaft ebyiri, shaft y'imbere no hanze. Ibikoresho bibisi bibarwa hagati yimbere numukanya.
TuribyizaPFR KILNAbatanga Ubushinwa.
Ibisobanuro bya tekiniki
Ibisohoka buri munsi: toni 300 kugeza kuri toni 600, kugeza 800tpd.
Lisansi: ifu ya coal, gaze karemano, gaze ya coke, gaze ya coke, gaze ihindura / isakoriya ivanze cyangwa andi makara avanze cyangwa andi makara atandukanye (1200KCal / NM3)
Ingano ya Limetine Ingano: 30mm kugeza 80m (nini, granular ntoya 1: 2)
Kunywa Ubushyuhe: Hagati ya 900 ~ 960KCal / Kg Lime
Gukoresha kw'imbaraga: munsi ya 35kwh / t lime
Lime quality: the activity >370ml (4nhci, iminota 5)
Loi munsi cyangwa ingana na 3%;

Annic Kilninzira yikoranabuhanga
Impfilar Shaft Imiterere yimbere kuva hejuru kugeza hasi ni pre -} kurikirana akarere,- gukurikiza akarere kabaka, no gukonjesha / gukonjesha / akonjesha / gukonjesha / akonjesha / gusebanya. Ibikoresho bibisi byerekanwe mbere, hanyuma byimurirwa hejuru ya kiln na hopori yumuzingo, hanyuma ugaburira umubiri wa kiln na marperitly. Preheated Ibikoresho fatizo byimukira muri zone yo hejuru ku itara ryumunywa n'ebyiri yishyuza aho ibikoresho fatizo bigira akamaro mu guhanura. Hafi ya-}} yuzuye muri zone yo hejuru yimukishwa mukarere gake, hanyuma ikajya kumanuka muri zone ikonje, hanyuma ikanyura muri zone ikonjesha, amaherezo ikanyura muri zone ikonje, amaherezo igabanuka kuri lime silo munsi ya kiln na lisher platifomu. Lime yuzuye yimuriwe mububiko na convoyeri.

Ibirangantego: Shaft Shaft Kiln, Ubushinwa, Abatanga, Abakora, Uruganda, Bakozwe mubushinwa